Projects
- 3 Finished
Search results
-
Finished
FFF - ACCEPT COST 536 - Alloy development for critical components of environmentally friendly power plants
Pein, C. (Contact person), Mayr, P. (Project manager), Holzer, I. (Contact person) & Cerjak, H.-H. (Project manager)
1/02/04 → 30/06/09
Project: Research project
-
Charakterisierung d Substruktur - Characterisation of the Substructure of Modern Power Plant Materials Using the EBSD Method
Sonderegger, B. (Project manager on research unit) & Cerjak, H.-H. (Attendee / Assistant)
1/03/03 → 28/02/04
Project: Research project
-
Computer simulation of precipitation kinetics in solid metals and application to the complex power plant steel CB8
Rajek, H. J. (Contact person) & Cerjak, H.-H. (Project manager)
1/07/01 → 1/11/04
Project: Research project